€35.00
Product | Discount | Coupon Code |
All Order | 3% OFF | TT3 |
1. The curing time is short, the mould process is not deformed, the surface of the finished product is smooth, the precision is high, and the shrinkage rate is low.
2. After curing, it has high hardness and certain toughness.
recommended printing time | 20-30s for bottom plate, 2.5-4.55 per layer (light intensity 300-40wuw/cm2) |
bottom lifting distance | 6 mm |
lifting distance | 6 mm |
bottom lifting speed | 60 mm/min |
lifting speed | 80 mm/min |
return speed | 150 mm/min |
absorption band | 385 ~ 410 nm |
1. moulding test environment and standards:
Temperature | 23 + 2C |
Relative humidity | 50% RH ± 5% RH |
Figure test spline standard | ASTM |
Post-curing conditions | put the test strips in water under 200mw/cm2 of 405-band uv rays and post-cure for 1 minute on the front and back sides. |
2. technical parameters after moulding:
maximum force (KGF) | 208.36 ± 10%. |
tensile strength (MPa) | 49.11 ± 10% |
deformation of the maximum force point (mm) | 5. 59 ± 10%. |
elongation at yield point (%) | 7.22 ± 10% |
elongation at break (%) | 10.00 ± 10% |
maximum flexural strength (MPa) | 61.17 ± 10% |
Bending modulus of elasticity (MPa) | 1346. 8 ± 10% |
Shore hardness (D) | 80 ~ 88 |
impact strength (J/m) | 50.13 ± 10% |
tensile modulus (MPa) | 498. 12 ± 10% |
Gewicht | 1 kg |
---|---|
Color | Black, Grey, White |